Nanoindentation of Natural Materials
Hierarchical and Functionally Graded Microstructures
Gebonden Engels 2018 1e druk 9781498784054Samenvatting
Nanoindentation of Natural Materials: Hierarchical and Functionally Graded Microstructures provides a systematic introduction and review of state-of-the-art statistical hierarchical and functionally graded structures found in bone, teeth, hair, and scales, from a nanoindentation perspective, including detailed microstructure and composition.
It covers the basics of hierarchical and functionally graded structures and nanoindentation techniques and detailed discussion with correlation micro/nano mechanical-structures
The book includes practical issues backed with experimental data
Specificaties
Lezersrecensies
Inhoudsopgave
Chapter 2: Nanoindentation of bone: a tough hybrid composite
Chapter 3: Nanoindentation of teeth: a hard but tough hybrid functionally graded composite
Chapter 4: Fracture toughness of enamel region: role of DEJ and modeling of fracture toughness
Chapter 5: Nanoindentation creep of enamel and dentin tissues
Chapter 6: Nanoindentation of hair fiber: a tough hierarchical layered architecture
Chapter 7: Nanoindentation of shell and scale: a hard-tough layered functionally graded hybrid composite
Chapter 8: Combined nanoindentation and finite element approach in hierarchical and functionally graded structures
Chapter 9: Conclusions
Rubrieken
- advisering
- algemeen management
- coaching en trainen
- communicatie en media
- economie
- financieel management
- inkoop en logistiek
- internet en social media
- it-management / ict
- juridisch
- leiderschap
- marketing
- mens en maatschappij
- non-profit
- ondernemen
- organisatiekunde
- personal finance
- personeelsmanagement
- persoonlijke effectiviteit
- projectmanagement
- psychologie
- reclame en verkoop
- strategisch management
- verandermanagement
- werk en loopbaan